Abstract

BethStar 60 steel plate is a high-strength product with a 60,000 psi minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability and formability. It provides the design engineer with a an economical high-strength low-alloy (HSLA) grade that can be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway haulers. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-421. Producer or source: Bethlehem Steel Corporation.