JESSOP ALLOY G is a nickel-chromium-iron-molybdenum-copper alloy exhibiting excellent resistance to a variety of corrosive conditions. It is resistant to both alkaline and acid environments, to stress-corrosion and to hot flue gases. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-337. Producer or source: Jessop Steel Company.