Abstract

BR-4 is a high-carbon high-chromium die steel with unexcelled abrasive-resisting qualities. It has important secondary hardening properties. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-460. Producer or source: Latrobe Steel Company.