Copper Alloy No. C33200 is a free-machining brass containing nominally 1.6% lead. Its machinability rating is 80% of that of Free-Cutting Brass. It has good resistance to corrosion in many environments. Alloy No. C33200 is used widely for general-purpose screw-machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-513. Producer or source: Brass mills.