Abstract

Copper Alloy No. C86100 is a copper-zinc-aluminum-manganese-iron alloy, sometimes classified as a high-strength yellow brass. The principal strengthening element is aluminum. Its tensile strength is typically 95,000 psi (655 MPa). It has a good combination of strength and ductility along with good resistance to corrosion. Its typical uses are marine castings, gears, gun mounts, bearing and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-510. Producer or source: Copper alloy foundries.