Abstract

BRUSH PHOSPHOR BRONZE is precision rolled and thermally treated to produce a material with consistent formability and properties. The product offers design advantages, improved service life and reduced fabrication problems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Cu-516. Producer or source: Brush Wellman Inc..

This content is only available as a PDF.
You do not currently have access to this content.