Abstract

STARK is a super high-speed steel having a very high carbon and vanadium content for exceptional abrasion resistance. It is well suited for premium cutting tools of all types, particularly those used for machining abrasive alloys, castings and heat-treated materials. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-441. Producer or source: Latrobe Steel Company.

This content is only available as a PDF.
You do not currently have access to this content.