INCO Alloy C-276 is a nickel-molybdenum-chromium-tungsten alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution control, industrial and municipal waste treatment, pulp and paper production, and other fields. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-311. Producer or source: Huntington Alloys.