Abstract
MONEL Welding Electrode 190 is used for shielded-metal-are welding of MONEL Alloys 400, 404, R-405 and K-500. It also is used for surfacing of steel. Dissimilar-welding applications for Welding Electrode 190 include joints between MONEL nickel-copper alloys and carbon steel, low-alloy steel, copper and copper-nickel alloys. It can be operated in all positions. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-310. Producer or source: Huntington Alloys.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International