BRUSH WELLMAN ALLOY 360 combines unique mechanical and physical properties required in high reliability electrical/electronic systems, heavy-duty controls, electromechanical devices and other high-performance applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Ni-326. Producer or source: Brush Wellman Inc..