Abstract

EASTERN STAINLESS TYPE 310S has high resistance to corrosion and oxidation at high temperatures. It also has high strength at elevated temperatures. Thus it is especially suitable for service at high temperatures. It is very ductile and can be welded readily. Among the many applications for Type 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-450. Producer or source: Eastern Stainless Steel Company.