Abstract

MUFLLER Alloy 6730 is a medium-leaded copper-base alloy with good machinability. It can be used with hard or soft mating members where moderate strength is sufficient. It can be joined successfully by soft soldering or silver soldering. Among its many uses are bearings, bushings, connecting rods and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-486. Producer or source: Mueller Brass Company.