Abstract

CARPENTER STAINLESS 302HQ-FM, a modification of Carpenter Stainless Custom Flo 302HQ, has excellent cold headability plus machinability approaching that of AISI Type 303 stainless steel. It is designed primarily for cold-headed parts that are to be drilled, slotted, broached, etc; in addition, it can be used in bar form on automatic screw machines on parts where thread rolling or cold form tapping operations are critical. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-432. Producer or source: Carpenter.