JESSOP JS600 is a nickel-chromium-iron alloy for use in environments requiring resistance to heat and/or corrosion. It has excellent mechanical properties and a combination of high strength and good workability. It performs well in applications with temperatures from cryogenic to more than 2000 F. Its many applications include aircraft/aerospace components, equipment for chemical and food processing and parts for heat-treating equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-287. Producer or source: Jessop Steel Company.