CRONIFER 1713 LCN is a fully austenitic low-carbon chromium-nickel-molybdenum stainless steel. It contains a nitrogen addition (0.10-0.20%) which helps to stabilize the austenite. Its molybdenum content (4.0-5.0%) provides good resistance to pitting attack by media containing chloride ions. Thus it has good resistance to brackish water and seawater. Typical applications are bleaching plants and equipment for handling aqueous chloride solutions. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-425. Producer or source: Vereingte Deutsche Metallwerke AG.