Abstract
Copper Alloy No. C61000 is an aluminum bronze containing nominally 92% copper and 8% aluminum. It is characterized by medium strength, medium ductility and a good capacity for being hot formed or cold worked. It has good resistance to corrosion. Its many uses include shafts, pump parts and bolts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Cu-458. Producer or source: Copper and copper alloy mills.