Abstract

GUTERL H-11 is a 5% chromium hot-work tool steel with an excellent combination of red hardness, shock resistance (toughness) and resistance to abrasion; these are the properties needed for good hot-work characteristics. It will withstand drastic cooling from maximum operating temperatures. Among the many uses for this steel are hot-die applications, structural parts for jet engines and missiles, extrusion mandrels and forging dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-412. Producer or source: Guterl Special Steel Corporation.