Abstract

PFINODAL C72900 is a copper-base alloy that derives its strength from spinodal hardening. It is produced by the manufacturer's wrought powder-metallurgy process for strip metal. This process provides the homogeneity and uniformity needed to achieve fully the available properties of the alloy system. Pfinodal C72900 is available in a variety of tempers. It is used for electronic connectors, switches and springs, especially for those requiring an exceptional combination of strength, thermal stability, formability and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-467. Producer or source: Pfizer Inc..