JESSOP JS825 is a wrought nickel-iron-chromium-molybdenum-copper alloy for use in extremely corrosive environments. The many corrosion-resistant properties of JS825 make the alloy a suitable choice for a variety of difficult applications. It is suitable for such applications as chemical and petrochemical processing, pulp and paper manufacturing, flue gas desulfurization systems and metal pickling operations. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-293. Producer or source: Jessop Steel Company.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Flue gas desulfurization systems
Corrosion-resistant alloys
Nickel-iron-chromium alloys
Chemical composition
Heat treatability
Joinability
Machinability
Workability
Elastic modulus
Tensile properties
Physical properties
Thermal properties
Chemical and petrochemical processing equipment
Pulp and paper processing equipment
You do not currently have access to this content.