Copper Alloy No. C41300 is brass with an addition of 1% tin. It has moderate strength and good ductility. It has a good combination of formability, joinability and resistance to corrosion. Typical uses comprise jewelry products, components for electrical switchgear, bushings and hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-430. Producer or source: Copper and copper alloy mills.