Abstract

AISI No. 664 is a nickel-base high-temperature alloy that can be precipitation hardened because of its contents of aluminum and titanium. Vacuum melting is used in its production to provide excellent quality and reproducability. It is used for applications requiring a good combination of creep and stress-rupture properties up to about 1500 F. Typical applications are gas-turbine components, airframes and fasteners. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-269. Producer or source: Nickel alloy producers.