Abstract
AMPCOLOY 712 is a medium-strength casting alloy. Its typical tensile strength is 60,000 psi in the as-cast condition. It has a good combination of strength, ductility and resistance to wear and corrosion. It is used widely for gears and formerly was known as Nickel Gear Bronze. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-420. Producer or source: Ampco Metal Inc..
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.