Abstract

CERROLOW-147 Alloy is a bismuth-base non-eutectic alloy that melts over the narrow, low-temperature range of 142-149 F (61-65 C). It has a slightly lower melting temperature than CERROBEND Alloy (Alloy Digest Bi-6, August 1978) and functions about as well for the same uses if its small freezing range is not objectionable. Cerrolow-147 Alloy provides engineers and technicians with an easily castable material that is ready for use as soon as it freezes. It is highly suitable in industry for such uses as anchoring parts for machining and support for bending tubing and extrusions. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, forming, heat treating, and machining. Filing Code: Bi-21. Producer or source: Cerro Metal Products.