Federated No. 7 is a lead-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Pb-1. Producer or source: Federated Metals Corporation, ASARCO Inc..