Abstract

Elektron TZ6 is a further variant of Elektron Z5Z having slightly higher tensile properties and also suitable for making castings which are subject to hot tearing. This alloy also has a very low tendency to microporosity and is weldable by the argonarc process. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Mg-10. Producer or source: Magnesium Elektron Ltd.