Abstract

Reynolds R301 is a composite material, constituted of a core of high strength aluminum alloy, clad with a corrosion-resistant aluminum alloy. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Al-16. Producer or source: Reynolds Metals Company.