Abstract

Rem-Cru C-130AM titanium-base alloy was developed with a minimum yield strength of 130,000 psi for fabrication into bars and forgings. It was formerly known as Rem-Cru RC-130B. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-3. Producer or source: Rem-Cru Titanium Inc..