Abstract

CARPENTER STAINLESS NO. 10 is a stainless steel developed to overcome the manufacturing difficulties associated with the rapid work-hardening of conventional 18-8 stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-14. Producer or source: Carpenter.