Abstract

AISI E52100 is a high-carbon, chromium alloy steel of the water hardening type. It has great depth hardenability and high wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: SA-16. Producer or source: Alloy steel mills and foundries.