Abstract

REFRACTALOY 26 is a high heat resistant alloy of nickel, chromium, cobalt and iron, possessing high creep and endurance strengths along with high ductility at elevated temperatures. It responds to precipitation-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-8. Producer or source: Westinghouse Electric Corporation.