Abstract

BELMALLOY is a high grade pearlitic malleable iron providing rigidity and shock resistance to high torque loads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: CI-6. Producer or source: Belle City Malleable Iron Company.