Abstract

HASTELLOY Alloy X is a nickel-chromium-iron-molybdenum alloy recommended for high-temperature applications. It has outstanding oxidation resistance at high temperatures under most operating conditions, and good high-temperature strength. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on forming, heat treating, and machining. Filing Code: Ni-14. Producer or source: Haynes Stellite Company.