Abstract
Copper No. C12100 is a silver-bearing copper deoxidized with phosphorus but with the phosphorus maintained at a low level (nominally 0.008%) to achieve good electrical conductivity. In the annealed condition it has low strength but can be cold worked to moderate strength levels. It is suitable for use in a wide range of electrical, architectural and hardware applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-402. Producer or source: Copper and copper alloy mills.
architectural applications, chemical composition, Copper alloy no. C12100, corrosion-resistant alloys, elasticity, electrical applications, electrical conductivity, fatigue properties, hardness, heat treatability, joinability, machinability, physical properties, shear strength, tensile properties, workability, UNS C12100
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Buildings and bridges
Electrical and electronics
Corrosion-resistant alloys
Copper alloys
Chemical composition
Electrical conductivity
Heat treatability
Joinability
Machinability
Workability
Elastic modulus
Fatigue properties
Hardness
Shear strength
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.