Abstract

HAYNES alloy No. 711 is a new, multicomponent hard-facing alloy that maximizes wear resistance with a minimum utilization of cobalt. Alloy No. 711 offers cost savings over the traditionally used cobalt-base alloys. It should be evaluated for general maintenance applicants such as a abrasion extruder screws, rock bits and slurry pumps. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-263. Producer or source: Cabot Corporation.