CERROCAST Alloy is a non-eutectic alloy with a melting range from 281 F to 338 F. It provides manufacturing engineers with an easily castable material that is ready for use soon after it freezes; moreover, it can be recovered readily and recycled into new uses any number of times. Cerrocast alloy is used widely for spray molding techniques, for sealing and soldering in low-temperature work, for proof casting in foundries and for masks in spray painting and electroplating. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: Sn-9. Producer or source: Cerro Metal Products.