Abstract
Inland INX Steels are a series of balanced composition steels with columbium or vanadium additions; they were developed to provide a choice of mechanical properties and engineering features. They are furnished to minimum yield point levels ranging from 42,000 psi (290 MPa) to 70,000 psi (485 MPa); this allows matching strength level to the job requirement. Their wide range of use includes automotive, tractors, farm equipment, bridges and buildings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-377. Producer or source: Ispat Inland Inc..