Abstract

AL Tech LMW-V is a molybdenum-type high-speed steel used extensively by domestic cutting-tool makers. It was designed to offer increased wear resistance while retaining the toughness characteristic of molybdenum-type high-speed steels. It is suitable for a wide variety of cutting-tool applications where improved resistance to abrasion is desired. Typical applications include twist dri milling cutters. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-353. Producer or source: AL Tech Specialty Steel Corporation.