Abstract

Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi. It has an excellent combination of strength and ductility along with good resistance to corrosion. Its numerous applications include cams, valve stems and marine hardware. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-365. Producer or source: Copper alloy foundries.