Abstract

ALLEGHENY LUDLUM AL-6X is an austenitic chromium-nickel-molybdenum stainless steel specifically designed for outstanding resistance to pitting and crevice attack in chloride-containing solutions. It possesses good ductility, high impact values and good weldability. It is an ideal material for condenser tubing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-349. Producer or source: Allegheny Ludlum Corporation.