Abstract

TECH-TRONIC 32 stainless steel is essentially a low-nickel chromium-manganese austenitic iron-base alloy. In the annealed condition it provides about twice the yield strength of AISI Type 304 stainless steel and almost the same resistance to corrosion. It also offers improved wear and galling resistance over standard stainless steels. TECH-TRONIC 32 can be cold worked to high strength levels with retention of good ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-348. Producer or source: Techalloy Company Inc..