BUNTING Alloy 935 is a cast bearing and bushing bronze. It has a good load capacity and excellent anti-friction characteristics. It is suitable for operating temperatures up to 450 F and has a wide range of applications in automotive, industrial and special equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-350. Producer or source: NL Industries Inc., Bearing Division.