Abstract

BELMONT ALLOY 2505 is a bismuth-base, eutectic, low-melting alloy. It melts at 158 F and provides engineers and technicians with an easily castable material that is ready for use as soon as it freezes. Alloy 2505 can be recovered easily and recycled into new uses any number of times. Its many uses include shuttle blocks, tube bending, chucks for lens buffing and grinding, anchoring, dies, and low-temperature solder. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Bi-9. Producer or source: Belmont Metals Inc..