Copper Alloy No. 175 is a wrought copper alloy that combines high strength with good electrical and thermal conductivities. It can be hardened by aging after a solution treatment. It is used for a variety of electrical hardware components and for industrial welding equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: Cu-333. Producer or source: Copper and copper alloy mills.