Abstract
FEDERATED F4110 is a general-purpose alloy for making intricate die castings. It is also used for thin-walled, complicated permanent-mold castings where maximum fluidity, pressure tightness and resistance to hot cracking are required. It has excellent castability and foundry characteristics, fair machinability and good strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-226. Producer or source: Federated Metals Corporation, ASARCO Inc..
cast aluminum alloys, castability, chemical composition, corrosion-resistant alloys, cracking resistance, die casting, elasticity, fatigue properties, FEDERATED F4110, fluidity, fracture toughness, hardness, heat treatability, joinability, machinability, physical properties, shear strength, tensile properties
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.