COLMONOY No. 22 is a nickel-base alloy supplied as atomized powder, welding rod and investment castings. The powder is applied with Colmonoy's FUSEWELD process to repair cast-iron parts. The investment castings are used in the glass industry as forming tools (plungers, baffles and sleeves) and as welding rod for repairing cast-iron glass-container molds and components. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion and wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: Ni-242. Producer or source: Wall Colmonoy Corporation.