Abstract

UNIFLUX V100 is a continuous flux-cored welding electrode (wire) that is used to deposit 1/2% molybdenum steel weld metal when used to weld 1/2% molybdenum steel for which it was developed. Welding is protected by a shielding atmosphere of 75% argon-25% carbon dioxide. This electrode is also used to weld other low-alloy steels and carbon steels; however, the weld metal may differ somewhat from 1/2% molybdenum because of weld-metal dilution. Uniflux V100 is used widely in shipbuilding to weld 1/2% molybdenum steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-339. Producer or source: Unicore Inc., United Nuclear Corporation.