Abstract

NIMAG 105 is a wrought nickel alloy with a high magnetostriction coefficient. It is easily formed or drawn, has a high Curie temperature and has low oxidation at high temperatures. It is recommended for electronic and electrical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-228. Producer or source: Spang Industries Inc..