NIMAG 100 is wrought nickel combining excellent mechanical properties with good corrosion resistance. It retains its strength to a high degree at elevated temperatures. Nimag 100 is produced by vacuum melting to provide close control of composition. It is used in a wide range of electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-224. Producer or source: Spang Industries Inc..