Abstract
ALUMINUM 295.0 is an aluminum sand casting alloy suitable for uses requiring high strength with ductility and toughness. It has fair castability, good machinability, and is used for a number of aerospace and automotive applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-222. Producer or source: Various aluminum companies.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Air and spacecraft
Automobiles and trucks
Corrosion-resistant alloys
Cast aluminum alloys
Aluminum alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Elastic modulus
Fracture toughness
Hardness
Ductility
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.