Abstract

DZR Yellow Brass is a new, corrosion-resistant brass. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, marine hardware, ornaments and door handles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-323. Producer or source: Federated Metals Corporation.